Hey all, I am having a problem with discoloration on the machined surfaces of aluminum die castings. These parts are cast from A383 aluminum alloy. The discoloration is kinda a brownish colored tint, maybe a tarnished look. If I scratch it with a knife blade, it is shiny underneath, so it is on surface only. It shows up randomly on different parts from different cnc machines. Maybe only 1 or 2 parts at a time. What could this be? Thanks for any thoughts on this.
25 years experience in aluminum die casting
25 years experience in aluminum die casting