I am working as a heat treatment engineer in one of the fastener company. 2 days ago, i saw something interesting. color of the waspaloy parts after heat treatment differed from each other( from purple to black) . Firstly i went to laboratory to check their mechanical and metallurgical properties. I took one part from each color. All values from the experiement showed us all the parts are okay. But i didnt understand how this occured.
My opinion was vacuum level, then i made an experiement. I put some waspaloy part to furnace without vacuum. After 16 hours at 760 C, ,i checked the parts. Results was interesting for me. All of the parts were black. I am really confused right now. Please help. Thanks.
I am working as a heat treatment engineer in one of the fastener company. 2 days ago, i saw something interesting. color of the waspaloy parts after heat treatment differed from each other( from purple to black) . Firstly i went to laboratory to check their mechanical and metallurgical properties. I took one part from each color. All values from the experiement showed us all the parts are okay. But i didnt understand how this occured.
My opinion was vacuum level, then i made an experiement. I put some waspaloy part to furnace without vacuum. After 16 hours at 760 C, ,i checked the parts. Results was interesting for me. All of the parts were black. I am really confused right now. Please help. Thanks.