Jul 18, 2001 #1 gdodd Automotive Joined Jul 18, 2001 Messages 138 Location AU Could someone tell me the nominal chemical composition for DIN 1652 C 45 Pb K + N. Thanks in advance Gdodd
Could someone tell me the nominal chemical composition for DIN 1652 C 45 Pb K + N. Thanks in advance Gdodd
Jul 19, 2001 #2 ghillis Mechanical Joined Mar 20, 2000 Messages 36 Location US Its a free cutting carbon steel, nominally AISI 1045 but leaded. I don't have exact composition, but... DIN - Norm 17210-84 --- 1.0504 K + N = Drawn and Normalized Hope this helps. Upvote 0 Downvote
Its a free cutting carbon steel, nominally AISI 1045 but leaded. I don't have exact composition, but... DIN - Norm 17210-84 --- 1.0504 K + N = Drawn and Normalized Hope this helps.
Jul 20, 2001 #3 welding1 Mechanical Joined Dec 2, 2000 Messages 122 Location GB I think its an obsolete standard C 45 is a carbon steel 0.42 to 0.5 carbon si<0.4 Mn 0.5 to 0.8% P and S less than 0.45 with lead additions of 0.2 to 0.3% Its material number is 1.0504 http://www.gowelding.com Upvote 0 Downvote
I think its an obsolete standard C 45 is a carbon steel 0.42 to 0.5 carbon si<0.4 Mn 0.5 to 0.8% P and S less than 0.45 with lead additions of 0.2 to 0.3% Its material number is 1.0504 http://www.gowelding.com