Does anyone know where to find a cross-reference between DIN material and ASME / ASTM material? Preferably FREE!
 
Werkstoff Number 1.4541
= DIN 17440 Type X6CrNiTi 18 10 (also seen as Type X10CrNiTi 18 9)
= Type 321 Stainless Steel
 