Bit of a long shot, maybe, but is anyone able to suggest a modern day equivalent to DIN17165 HII boiler plate material. The material specification is called up quite clearly on a vessel fabrication drawing circa 1967, but I have drawn a blank so far in finding any mention of this material in all the normal references. I am aware of DIN17155 HII but even with my "old" eyes I can spot a 6 when I see one !!

Many thanks in anticipation of your replies.

 
Replies continue below

Recommended for you

DIN 17155 was replaced in 1993 by EN 10028-2.
P265GH according EN 10028-2 is nearly identical to HII.
An equivalent ASME-material is SA 516 Grade 60
 