I'm looking for the dimensional specs on 28" pipe. Specifically, I need the bore (I.D.) of 28" SCH-40s (STD) pipe. Any ideas?
Tks all-
C. Fee
 
My Mechanical Engineering Handbook gives the I.D. of standard weight 28" steel pipe as 27.250" (wall thickness = 0.375"), but doesn't show this as Schedule 40. There is no Schedule 40 listed for 28" dia.
 
Maury & PiperAnton -
BIG thanks !
C. Fee
 
My Machinery Handbook shows for:
24" 22.624"ID .688"wall
32" 30.624"ID .688"wall
Properties of American National Standard Schedule 40 Welded and Seamless Wrought Steel Pipe