This may be a basic question but, I am fairly new to welding chemical analysis.
I am using an XRF spectrometer to measure weld deposit on a 3/4" NPS A182-TP316L socket weld (as per client specs).
I am wondering what code and table the analysis should conform to.
Section II Part A is for Pipe and fittings, Section II Part C is for Undiluted Weld Deposit, and Section IX A number 8 is for procedure qualification.
I don't know which is applicable to the completed weld in this case.
Thanks
I am using an XRF spectrometer to measure weld deposit on a 3/4" NPS A182-TP316L socket weld (as per client specs).
I am wondering what code and table the analysis should conform to.
Section II Part A is for Pipe and fittings, Section II Part C is for Undiluted Weld Deposit, and Section IX A number 8 is for procedure qualification.
I don't know which is applicable to the completed weld in this case.