Dear Cobra17
see UW-28(c)
(c) The procedure ....
(1) When the welding process is manual, ....
Yes,Weld a insulation support pins on vessel is manual.
(2) When the welding is ....
Weld a insulation support pins on vessel is not automatic welding process.
see PW-28.1.2
Except as provided in (a) and (b), the
Welding Procedure Specification, the welders and the
welding operators used in welding nonpressure-
bearing attachments which have essentially no load-
carryingfunction(such as extended heattransfer surfaces,
insulation support pins, etc.) to pressure parts shall be
qualified in accordance with Section IX. Possession of a
Certificate of Authorization by the organization
performing such welding is neither required nor prohib-
ited.
(a) When the welding process is automatic, ....
(b) When the material used for the nonpressure part
makes the mechanical test requirements for procedure
qualification and performance qualifications impractic-
able (i.e., insufficient material ductility), a weld test
coupon may be evaluated using the macro-examination
method for both groove and fillet welds. The test
coupon may be of production configuration and shall
be of sufficient length to contain a specimen for
macro-examination. One face of the cross-section shall
Should we follow this requirement?