Dear all,
Consider this situation an 8mm P1 plate welded against a 20mm P1 plate. Then the base metal qualified thickness range is 1.5 - 40mm and the deposited weld metal thickness qualified "t" is only 16mm. My question is what is the benefit of preparing a procedure so?
By using that procedure we can't deposit weld metal more than 16mm and the Base metal thickness qualified is 1.5 to 40mm
 
There must be some key information you are not sharing with us.

For example, the WPS could have been qualified using more than one welding process or more than one F number. That being the case, each process or F number used during the qualification effort would have a specific thickness range for which it is qualified based on the thickness of the weld deposit (t). The combination of welding processes or F number would be qualified for a thickness range based on the thickness (T) of the test coupon recorded by the PQR when the procedure was qualified.

Best regards - Al
 
Putting a thin overlay on a thicker piece of material is typically where these types of procedures come into play.


Quality is not an act, it is a habit - Aristotle
 
You should ask the originator of the WPS, why he/she did so. In the distant past, I did see his type of PQR usd to qualify a procedure to two different Codes, one being ASME IX.
 