Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Difference between generalized and localized cracking

Status
Not open for further replies.

victorzv

New member
Joined
Apr 13, 2007
Messages
16
Location
CA
The question may be stupid, but I cannot find any clear definition of both generalized and localized cracking.

Does anybody know the difference, preferably in aircraft structures?
Thank you.
 
localised cracking is an isolated crack, say a crack at a hole. typically initiated by a specific (individual) flaw.

generalised cracking is several cracks reasonably close together, or multi-site damage. typically initiated by fatiguing many small (minor) flaws that are replicated at many sites (ie typical manufacturing quality).
 
Thank you rb1957!

May I say that cracks found in a joint or fitting (where we have significant load transfer from fastener to fastener) are localized, while cracks found at a wing skin panel spanwise splice (load transfer is almost zero) are generalized in terms of the wing fatigue life?

Or you think my interpretation is irrelevant?
 
i wouldn't connect the terms with load transfer. splices with load transfer are just as likely to develop generalised fatigue cracking as those without load transfer.
 