I'm working at a heat recovery exchanger connected in line with an CH4 engine .
the fisrt exchanger will have inlet temp 440° and outlet temp 120°C
The inlet temperature will be 120°C and outlet 50°C.
I'm selecting the tubes material and i'm considering AISI316L
but a some source insist for AISI 316 Ti.
What the real difference in such a corrosion enviroments between these materials ?
thank you in advance !!