Hello first time making battery most likley i choose wrong BMS.
1 wire too much.
IMG_20200910_192334_dav1vx.jpg
BATERIJA_3D_eqixij.png
bat4444_hvl19t.png
laidaixxx_uxozir.jpg



which bms i should choose ? thank you!

Untitled888_w0ciif.png
 
Usually you can run a few less batteries than the BMS capacity. Some BMSes have you skip the bottom cell lead some the top and I've even seen some have you skip specific middle ones.
I'm not sure on the Daly BMSes.

Why not write the company. They answer quickly and will give you a definitive answer.



Keith Cress
kcress -
 
Tiz the industry standard IR. They are only there to sense the cell potentials so they feed high impedance inputs.

Though the big current leads and even the FETs are indeed usually a joke with respect to the actual current ratings.

Keith Cress
kcress -
 
Thank you for answers! i contacted supplier. when i solve this i will share it here maybe its gonna be usefull for someone else
 