Developing Heat Resistant Steels

Status
Not open for further replies.

Robertmet

Materials
Aug 5, 2007
153
I found this article confusing and wondered if anyone could explain it.The presentation was this morning so perhaps something will show up.
 
Replies continue below

Recommended for you

Robertmet, I too join you. 500C is not sufficient to change the interatomic distances nor break the bonds.

"The scientists found that magnetic fluctuations which occur at atomic level give rise to fundamental changes in the strength of the steels. "

I hope someone here is able to give us a better insight.



Chocolates,men,coffee: are somethings liked better rich!!
(noticed in a coffee shop)
 
The only thing I could guess at is the transformation of some steels from ferrite to austenite (thus affecting its magnetic properties, and strength properties) at higher temperatures...which, if it is what they are discussing, is a great big "duh" to most engineers.
 