1) Double-Welded Butt Joint (Type 1)
E
1.1 Full RT --> 100%
1.2 Spot RT --> 85%
1.3 No RT --> 70%
2) Single-Welded Butt-Joint (Type 2)
(Backing Strip in place)
2.1 Full RT --> 90%
2.2 Spot RT --> 80%
2.3 No RT --> 65%
3) Single-Welded Butt-Joint (Type 3)
3.1 No RT --> 60%
Note, equivalent welds to item 1.1 above include Single-Welded Butt-Joint back chipped and welded from the inside;
those may have 100% joint efficiency.
Weld Categories A, B, C, D (UW-3)
A --> Longitudinal Seams
B --> Circumfrential Seams
C --> Terminal Weld end in a flange
D --> Attachments
Type of Radiography
RT-1 --> Full lenght, full radiography of a;; butt welds
(except >= NPS 10 or tn >= 1 1/8"
RT-2 --> Cat-A: Full Lenght
Cat-B: T-joints
RT-3 --> Spot Radiography (UW-52)
RT-4 --> Partial / No Radiography
Seamless Heads & Vessel Sections --> 100%
Piping SAW & Seamless --> 100% ERW --> 85%