For health & environmental reasons we are considering using water based specialised detergents to degrease high strength aerospace materials like aluminium 7075 & marage steel used for critical applications. We are concerned about the detergents possibly causing SCC and/or embrittlement. The materials are typically cold/hot worked and in the case of the steel, welding is also done. Cleaning with the detergent will always be followed by a de-ionized water rinse/spray-off.
The suppliers of the detergents are quite protective about their formulations and we do realise the proper way would be to do extensive testing.
Would appreciate if anybody has any experience to share on the above. Any successes stories?
Thanks