Deposited 't' thickness

Status
Not open for further replies.

DVWE

Petroleum
Apr 5, 2007
2,317
I have a test coupon 1.25" in thickness. I have deposited .5" of SMAW, .25" GMAW, and .5" of SMAW respectively (GMAW is between SMAW depositions). Is my deposited weld metal thickness (t) for SMAW per QW-451, .5" or 1"?

Thanks in advance.
 
Replies continue below

Recommended for you

The qualified deposited thickness should be 1", considering that is what was actually deposited into the weld area.
 
My question is why would you run your test plate that way?
 
There was a misunderstanding between the production supervisor and me. I originally asked for a single V and since 90% of our production joints are double V, that's what they did.
 
You have 1" of deposited weld metal with the SMAW process. We have often qualified our proceures this way on heavy wall items.

 
Gents (&ladies?),

Thanks for the replies. I was the only one making an issue of this, as everyone I've talked to says the same as you all have said.
 