Thanks for all .
The alloy are CD3MN and CE3MN.
The nitrogen content is .19 and it's adding whit Iron Chromiun Nitro during the melting.
I use magmasoftware to calculate the risering sistem but doesn't work. I concluded that the módulus of sleeves must be the doble than the others alloys.
The deoxidation is a bit of Al, FeSiZr, CaSiMn, Mish, NiMG, Ti and Se. Is there difference to use the deoxidants at ladle instead during the tapping.
A lot of thanks