Hello every one,
The exchange tube bundle was found with one tube has been damaged; seems to be during handling & transportation; two dents has been observed. NDT LPI "liquid penetrate Inspection” was conducted and showed no indication of cracking. Impact area caused a dent within damaged area measuring ~ 10mm long x 7mm wide x 1.7mm deep. At the impact point pipe section became out of round and the dents bend containing a scratch, gouge, or groove.
However, our construction code is ASME B31.3 process piping and there is no recommendation for this case. Can I apply ASME B31.4 code or ASME B31.8 recommendations??!!
I prefer this tube to be plugged.
Your comments suggestions would be greatly appreciated
Zayed
Exchanger Specifications:
M.A.W.P. (Tube side): 330 psi @ 600F
M.A.W.P. (Shell side): 190 psi @ 650F
Tube Material: SA-214
Outside Diameter/Thickness: 19.05 mm/2.16 mm (Tmin 1.5 mm min)
The exchange tube bundle was found with one tube has been damaged; seems to be during handling & transportation; two dents has been observed. NDT LPI "liquid penetrate Inspection” was conducted and showed no indication of cracking. Impact area caused a dent within damaged area measuring ~ 10mm long x 7mm wide x 1.7mm deep. At the impact point pipe section became out of round and the dents bend containing a scratch, gouge, or groove.
However, our construction code is ASME B31.3 process piping and there is no recommendation for this case. Can I apply ASME B31.4 code or ASME B31.8 recommendations??!!
I prefer this tube to be plugged.
Your comments suggestions would be greatly appreciated
Zayed
Exchanger Specifications:
M.A.W.P. (Tube side): 330 psi @ 600F
M.A.W.P. (Shell side): 190 psi @ 650F
Tube Material: SA-214
Outside Diameter/Thickness: 19.05 mm/2.16 mm (Tmin 1.5 mm min)