Hi;
I need to get a "density as a function of temperature" chart or equation from room T (70 F) to melting point (2500 F), if it exists. I'm not looking for a particular classification of steel yet, because I first want to get something representative of a welding situation (weldable material, mild steel).
Bibliographic or web-based references would be greatly appreciated.
Regards
 
Replies continue below

Recommended for you

VinceFabspec;
You can try to Google this information, first. I suspect it won't be easy to find.

One source that I have is in Appendix B of "Transportation Phenomena in Materials Processing" by Poirier and Geiger. It lists density at selected temperatures for limited carbon steels, stainless steels and nonferrous alloys.
 
Hope this help,

data for general steels :

densityos2.jpg


Stan
 
stanislas,
For temperatures below 15 deg C, can we interpolate the curve (assuming it linear)?
Cheers,
gr2vessels
 
Thanks a lot Stan;
is it possible to get the reference of this graph, I would like to get a closer look to these results.
Regards
 
density can easily be calculated if you have thermal expansion coefficient for the material in the temp range
the total mass is constant and volume changes with temp.
 
Ok;
I can simplify my problem by using the thermal expansion coefficient.

For further evaluation I want to represent the linear (and later the volumetric) dimensional change of an element during the different change of phase and structure (for a chosen steel chemistry):
- Does the density change depending on the phase?

STANISLASDZ, can you give me the reference for the graph above, I would really appreciate!

Regards
 
VinceFabspec ....i haven't exactly the reference of this curve.

For better informations see the ASM handbook Vol 1

 