Delrin AF (15% PTFE filled delrin) is often used (tapped)to make nuts for precision metal leadscrews on small mills and lathes. Would it not be best to simply use pure (teflon)PTFE? What about UHMWPE? Its apparently has similar properties to teflon but less resistant to abrasion.

The goal is, the tightest fitting nut with the least friction/stiction. Delrin AF definitely beats brass for fit and wear but Im curiuos if teflon or UHMWPE are even more suitable.


 
Replies continue below

Recommended for you

Delrin is very strong. PE and PTFE are quite weak in comparison. The threads might not wear, but they might strip or be cut by harder particles.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor