Hi all,
I have problem with my HDPE flange.
There are some defects found on the flange surface of HDPE Flange.
What is the acceptance criteria to asses the defect??
As i know, for metallic material we can refer to ASME PCC-1,but i dont know for non metallic material.
Thanks.
I have problem with my HDPE flange.
There are some defects found on the flange surface of HDPE Flange.
What is the acceptance criteria to asses the defect??
As i know, for metallic material we can refer to ASME PCC-1,but i dont know for non metallic material.
Thanks.