I'm designing a deck with the following specs:
Height: > 30" above ground
Material: Western Red Cedar (No. 2)
Fb = 575 psi
Fv = 65 psi
Fc (perp) = 350 psi
Fc (parallel) = 825 psi
E = 1.1E6 psi
Joist size: 2x6
I need to come up with a detail for the deck-railing post connection that meets the load requirement in the IRC (R301.5) of 200 lbs.
I have looked at using a Simpson Strong-Tie HD2AHDG deck post connector, however this requires a 2x8 joist size. I also looked at using a DeckLok bracket system. I didn’t see anything on their website ( regarding joist size requirement (or type of wood).
Does anyone have any experience with the DeckLok brackets, or do you have any suggestions for a detail I could use for the post connection that will meet the code requirement?
Thanks for your help!
Height: > 30" above ground
Material: Western Red Cedar (No. 2)
Fb = 575 psi
Fv = 65 psi
Fc (perp) = 350 psi
Fc (parallel) = 825 psi
E = 1.1E6 psi
Joist size: 2x6
I need to come up with a detail for the deck-railing post connection that meets the load requirement in the IRC (R301.5) of 200 lbs.
I have looked at using a Simpson Strong-Tie HD2AHDG deck post connector, however this requires a 2x8 joist size. I also looked at using a DeckLok bracket system. I didn’t see anything on their website ( regarding joist size requirement (or type of wood).
Does anyone have any experience with the DeckLok brackets, or do you have any suggestions for a detail I could use for the post connection that will meet the code requirement?
Thanks for your help!