Jul 19, 2024 #1 Akoll Mechanical Joined Jun 20, 2023 Messages 15 Location IQ Dear All, which standard and level applicable for UT , for Forged Ring A105N OD 1580mm , ID 1275 mm and Th260 mm . Please advise which standard is applicable to do such test (UT)?
Dear All, which standard and level applicable for UT , for Forged Ring A105N OD 1580mm , ID 1275 mm and Th260 mm . Please advise which standard is applicable to do such test (UT)?
Jul 19, 2024 #2 Stick. Mechanical Joined Feb 20, 2019 Messages 280 Location US I believe ASTM A388 would be a relevant standard for UT. Upvote 0 Downvote
Jul 19, 2024 Thread starter #3 Akoll Mechanical Joined Jun 20, 2023 Messages 15 Location IQ what about this ASTMA578/A578MLEVELC ? Upvote 0 Downvote
Jul 19, 2024 #4 EdStainless Materials Joined May 20, 2004 Messages 16,398 Location Waukesha WI USA Which is listed in the material specification? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed Upvote 0 Downvote
Which is listed in the material specification? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed
Jul 19, 2024 Thread starter #5 Akoll Mechanical Joined Jun 20, 2023 Messages 15 Location IQ Not listed in the materials specification Upvote 0 Downvote
Jul 20, 2024 #6 EdStainless Materials Joined May 20, 2004 Messages 16,398 Location Waukesha WI USA So there is no specification? Start by looking at ASTM casting specs for the same material and seeing what they refer to for NDT. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed Upvote 0 Downvote
So there is no specification? Start by looking at ASTM casting specs for the same material and seeing what they refer to for NDT. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed
Jul 20, 2024 #7 mfgenggear Aerospace Joined Jan 23, 2008 Messages 3,663 Location US This https://www.astm.org/a0388_a0388m-19.html Upvote 0 Downvote