Dear All,
which standard and level applicable for UT , for Forged Ring A105N OD 1580mm , ID 1275 mm and Th260 mm .
Please advise which standard is applicable to do such test (UT)?
 
Replies continue below

Recommended for you

I believe ASTM A388 would be a relevant standard for UT.
 
what about this ASTMA578/A578MLEVELC ?
 
Which is listed in the material specification?

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Not listed in the materials specification
 
So there is no specification?
Start by looking at ASTM casting specs for the same material and seeing what they refer to for NDT.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 