I have three materials at hand, JIS-SS400, Q435, and Q235 all for a basic structural application. The vendors supplying the steel have been less than cooperative thus far.
I have yet to find any information other than their basic composition tying them to a UNS number or ASTM equivalent. Am I looking at having to qualify new procedures to allow our guys to weld on any of these per D1.1, or is there any literature out there with the equivalents of these steels that will allow me to use our prequalified procedures?
Thanks in advance.
I have yet to find any information other than their basic composition tying them to a UNS number or ASTM equivalent. Am I looking at having to qualify new procedures to allow our guys to weld on any of these per D1.1, or is there any literature out there with the equivalents of these steels that will allow me to use our prequalified procedures?