D1.1 code book 2010 version

Status
Not open for further replies.

dbernard2012

Petroleum
Jan 14, 2014
10

RE; Table 2.9. Can someone explain this table? question below.

Question : What is the Z loss dimension for pre-qualified PJP T-,Y-K-
Connector what a groove angle of 50 degrees using short circuiting transfer GMAW in the horizontal position?
 
Replies continue below

Recommended for you

Did you look at the clause and the figures that are referenced? The figures on the last page of clause 3 pretty much says it all.

Best regards - Al
 