RE; Table 2.9. Can someone explain this table? question below.

Question : What is the Z loss dimension for pre-qualified PJP T-,Y-K-
Connector what a groove angle of 50 degrees using short circuiting transfer GMAW in the horizontal position?
 
Did you look at the clause and the figures that are referenced? The figures on the last page of clause 3 pretty much says it all.

Best regards - Al
 