Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JAE on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Cutting tantalum

Status
Not open for further replies.

BeliefMakr

Industrial
Joined
Jul 24, 2005
Messages
4
Location
US
We have a 2000Watt CO2 laser and have been asked to try and cut tantalum. I don't know what specifications the metal will be (IE: thickness or shape). Given what little information I have, does anyone know what type of cutting conditions I could try? What assist gasses work best? Cutting speeds? I haven't recieved any material yet and I don't want to waste it experimenting.
 