Pavel Zemanec
Industrial
Dear all,
I would like to ask you for your help / tips. We have very simple task but unfortunatelly limited budget :-(
We would need to cut from very thin textile (0,1mm) two simple shapes - see attached drawings and pictures. Required cycle time: max. 30 s / 1 cutted piece.
We tested CO2 laser - 30W and the result was good but this solution was not approved by our customer because of high costs. Would you have any tips for this task? Our idea is to cut the complete shape with some stamp where some hot wire in the required shape could be integrated. Maybe we would need to use special teflon surface in order to avoid sticking etc. Does anybody have any experience with such a solution or do you know about similar technology / application?
Thank you very much for your help
I would like to ask you for your help / tips. We have very simple task but unfortunatelly limited budget :-(
We would need to cut from very thin textile (0,1mm) two simple shapes - see attached drawings and pictures. Required cycle time: max. 30 s / 1 cutted piece.
We tested CO2 laser - 30W and the result was good but this solution was not approved by our customer because of high costs. Would you have any tips for this task? Our idea is to cut the complete shape with some stamp where some hot wire in the required shape could be integrated. Maybe we would need to use special teflon surface in order to avoid sticking etc. Does anybody have any experience with such a solution or do you know about similar technology / application?
Thank you very much for your help