Oct 12, 2022 #1 Thanh Tran Industrial Joined Jan 7, 2021 Messages 33 Location US Hi, our company has a Mitsubishi CO2 laser, model 3015LVP-40CFX. I try to cut 0.047” galvanized material. What cutting condition can I use? Thanks
Hi, our company has a Mitsubishi CO2 laser, model 3015LVP-40CFX. I try to cut 0.047” galvanized material. What cutting condition can I use? Thanks
Oct 13, 2022 1 #2 drossfree Materials Joined Apr 10, 2008 Messages 108 Location CA you can use stainless steel condition for the same thickness but cut your speed in half. there will be burr on the bottom but it will cut Upvote 0 Downvote
you can use stainless steel condition for the same thickness but cut your speed in half. there will be burr on the bottom but it will cut