Cutting Force Calculation

Status
Not open for further replies.

Auspex

Mechanical
Jan 20, 2005
29
Can anyone point me to a good resource for calculating cutting force on a tool insert? Even a plot or measurement would be a good starting point.
 
Replies continue below

Recommended for you

Machinery's Handbook has a great second on cutting forces and chip flow angle.

Heckler [americanflag]
Sr. Mechanical Engineer
SWx 2007 SP 4.0 & Pro/E 2001
o
_`\(,_
(_)/ (_)

"Avoid the base hypocrisy of condemning in one man what you pass over in silence when committed by another." -- Theodore Roosevelt
 
Machinery's Handbook has equations for estimating cutting power and force required for metal cutting. Cutting force normal to the cutting can be calculated from the power required ( Power = "RPM" x force x radius.
 
Wow the Kennametal site is cool, bookmarking that one now. Thanks guys, should have thought to check the Machinery's Handbook......pretty much the answer to everything in there :)
 
Hi,
also try to google for "Pijspanen" and "Ernst-Merchant" theories.

Regards
 