We have to cut a small section (about 3 feet) of our non-seggregated 10 kV bus bar (all three phases) since the ends are not aligning with the bar holes at the generator end (other end of the bus bar is connected to the transformer low voltage bushing stubs). Instead of cutting the bar at the end and machining new holes, we want to cut it in the middle and reconnect it (bolt or weld). The alignment issue came because of wrong calculation on dimension (this is a new installation).
Does anybody see any problem with cutting the middle section of the bus bar and reconnecting it?
Much appreciated.

 
Copper is a nightmare to weld, especially in the field, which from a practical point of view leaves you with making a bolted joint. A bolted joint is never going to be as good as a solid bar, which is what you would have if you drilled the bar end. Is it a particularly awkward task to drill the bar?



----------------------------------
image.php

If we learn from our mistakes I'm getting a great education!
 
Copper or aluminum?
IPS?

Bill
--------------------
"Why not the best?"
Jimmy Carter
 
Good point Bill, aluminium would be a lot easier to deal with. Oops!


----------------------------------
image.php

If we learn from our mistakes I'm getting a great education!
 
one thing i had done with the same problem last year that joint the two bus bar segment with flexiable bar but the section was of ngr,in case of outgoing which carry havey current, any patch give you local heating

 
At 10 kV, regardless of how simple it looks, have a professional switchgear manufacturer how deals with medium voltage gear assembly do the job. The stated approach sounds too causal to me.

Rafiq Bulsara
 
Sounds like a potential source of local PD activity.
 
Thanks all for the answer. It is copper bus by the way.
 