Dear All.
My fabricator installed 4 lifting lug on the 4m OD vessel with weight about 40MT. However the End User question (rejected) about curvature of the reinf pad for lifting lug, the curvature seem "bulged" due to the manual pressing forming. The "bulge" curvature height by 4.1mm from the outer shell curvature of the vessel.
My questions
1) How to determine the safety of the lug if bulge in question?
2) Where to get the "acceptance criteria" of the curvature
3) How to do NDE to determined the strength of reinf pad
We aware the curvature of the structure increased strength.
Any help please
Thanks
My fabricator installed 4 lifting lug on the 4m OD vessel with weight about 40MT. However the End User question (rejected) about curvature of the reinf pad for lifting lug, the curvature seem "bulged" due to the manual pressing forming. The "bulge" curvature height by 4.1mm from the outer shell curvature of the vessel.
My questions
1) How to determine the safety of the lug if bulge in question?
2) Where to get the "acceptance criteria" of the curvature
3) How to do NDE to determined the strength of reinf pad
We aware the curvature of the structure increased strength.
Any help please
Thanks