French copper cure test - I have two(2) lab ovens and using oven A the results from the cure test or OK however using Oven B the same profile sample sometimes show "dark" indicating the profile is not completely cured / or there is sulfar still present?
In a first moment you need to check if the temperature profile are the same on the ovens, without this information is very difficult to give your a feedback and solution.