Has anybody had any experience with overlaying CuAl-A2 on a Nitronic 60 base? My thoughts are that it should be relatively straight forward welding, similar to overlaying CuAl on 300 series stainless, but its always worthwhile to ask if there might be some unforseen issues.
 
Replies continue below

Recommended for you

We have overlayed aluminum bronze on 316 stainless steel impellers with the GTAW process without incident.

 