Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Cryogenic Treatment of Materials

Status
Not open for further replies.

weed78

Mechanical
Joined
Mar 24, 2006
Messages
13
Location
CA
I tried this posting in the Cryogenic Engineering forum but received no replies so I will ask my question here.

Is there a significant difference in the final wear properties of tool steel materials cryogenically treated in liquid vs vapor?
 
You probably mean the Subzero treatment used to transform retained austenite (obtained upon quenching in oil or in air) into martensite (to be subsequently tempered) in order to increase the hardness of the steel.
What matters is the temperature.
You might use dry ice (frozen carbon dioxide) at -78.5 C or
liquid nitrogen at -196 C.
It depends on the amount of austenite present and on its stabilization, that may make it harder to transform.


 
We usually triple cryo for our machine tool parts. This is to reduce distortions for later temperature variations. I have never seen any part in contact with the liquid nitrogen, the tray is suspended in the boiling zone and heat is removed there. Recently we began qualification of an in-house cryo at -100°C, becuase this is the lowest temperature our freezer can maintain...
 