I am contemplating a fixture that uses an aluminum strip to crimp a stainless steel wire. Would there be an issue with using two different metals?
 
The aluminum strip will wear much more than the wire you are trying to crimp. Any thoughts on using a tool steel to crimp the stainless?

"Art without engineering is dreaming; Engineering without art is calculating."

Have you read faq731-376 to make the best use of these Forums?
 
This fixture will be in a fairly corrosive environment. I need to stay with stainless and/or aluminum. I am choosing stainless for the wire because it needs to be formed into a rigid shape. I am thinking of aluminum to crimp because of malleability.
 
" I am thinking of aluminum to crimp because of malleability. "

Um, yeah. Meaning it's going to deform if you try to crimp/bend stainless wire with it. If that is what you intend, fine, but then you are probably doing more crimping of the aluminum? I think there is some misunderstanding between what you wrote and what we-all are reading here. A sketch or picture could help a lot.
 
hi skuntz

Mixing aluminium and stainless together could generate galvanic corrosion if any electrolyte is present between the two materials.

desertfox
 
All materials corrode or degrade, it's just a matter of how quickly due to conditions.

What is the material and material condition being crimped? And also, what is the nature of the corrosive environment?
 