Feb 8, 2005 #1 Mike00 Civil/Environmental Joined Jun 19, 2004 Messages 13 Location US Hello, Does anyone know where I can find data on creep behavior of Froth-pak and Handi-Foam? I've tried their respective websites, but have had no luck. Thanks,
Hello, Does anyone know where I can find data on creep behavior of Froth-pak and Handi-Foam? I've tried their respective websites, but have had no luck. Thanks,
Feb 8, 2005 #2 Ron Structural Joined Sep 24, 1999 Messages 16,336 Location US In general, these are materials that shouldn't received loading that would cause creep. Upvote 0 Downvote