i have constructing one hospital 11 storied building at mumbai.
i am facing cracks problems at concrete
in every pouring after five hours the concrete surface is showing cracks ( specifically in slabs )
Width of cracks maximum 6MM
Depth of cracks 20 to 30MM
The thickness of RCC slab is 150MM
Reinforcemet used per Cum : 140 Kg
Area covered per pouring time : 1000 Sqm.
Please give the information to avoid such type of problems.