corrosionman
Mechanical
We have an open topped circular tank and the base is a steep sided cone. It is a settlement tank where the heavy solids sink and get drawn off at the base and clarified liquid overflows into a channel at rim level. Tank dia is 25 feet and total height approx 30 feet. Temp ranges from ambient
to 60 C. Tank is 6 mm mild steel. Contents vary daily from slightly acid to slightly alkali. Tank has some protective lining but it is in poor condition. There is no turbulence or vibration - - - it is a very gentle flow .
A small support bridge was WELDED from side to side at rim level. Soon after we noticed cracks down the wall (approx at 45 degree) going out from the new welded points.
The vessel is 12 years in present location , but it had prior use in an unknown situation.
i.e. A second hand tank !
What can be cause of these cracks.
Any comments much appreciated.
to 60 C. Tank is 6 mm mild steel. Contents vary daily from slightly acid to slightly alkali. Tank has some protective lining but it is in poor condition. There is no turbulence or vibration - - - it is a very gentle flow .
A small support bridge was WELDED from side to side at rim level. Soon after we noticed cracks down the wall (approx at 45 degree) going out from the new welded points.
The vessel is 12 years in present location , but it had prior use in an unknown situation.
i.e. A second hand tank !
What can be cause of these cracks.