Cracks occurred in a slab that was placed per drawings, protected & consolidated per ACI, everything was performed by the book.
The 8" slab is on grade with grade beams placed at 21'oc and saw joints at 10'6. The slabs were required to be placed in lanes no greater than 25' in width. The cracks have occurred about 2' to 3' off the grade beams and are approx. 0.012 to 0.020. The cracks dont appear to be very deep. The base is select fill with 8" of small gravel under a 15 mil vapor barrier.
The design mix was an approved mix with HRWR which allowed up to a 8" slump and 5% air. My second placement I took the HRWR out and went to a 5" slump and reduced the air to 3%. This seems to have help but not totally convinced that this was the problem.
I have read through all the ACI books trying to understand the type of crack. It doesn't appear to be shrinkage but more of a stress crack. The specifications states no cracks of any size will be allowed. Supposedly this is why I'm forced to place the concrete in 25' x 100' lanes, yet cracking still occurred.
Does anyone have a suggestion what may have caused this? I have about 50 more of these lanes to place and dont want the same problem.
The 8" slab is on grade with grade beams placed at 21'oc and saw joints at 10'6. The slabs were required to be placed in lanes no greater than 25' in width. The cracks have occurred about 2' to 3' off the grade beams and are approx. 0.012 to 0.020. The cracks dont appear to be very deep. The base is select fill with 8" of small gravel under a 15 mil vapor barrier.
The design mix was an approved mix with HRWR which allowed up to a 8" slump and 5% air. My second placement I took the HRWR out and went to a 5" slump and reduced the air to 3%. This seems to have help but not totally convinced that this was the problem.
I have read through all the ACI books trying to understand the type of crack. It doesn't appear to be shrinkage but more of a stress crack. The specifications states no cracks of any size will be allowed. Supposedly this is why I'm forced to place the concrete in 25' x 100' lanes, yet cracking still occurred.
Does anyone have a suggestion what may have caused this? I have about 50 more of these lanes to place and dont want the same problem.