Bobfoam
Materials
- Jul 11, 2006
- 4
Hello everyone,
I have been working on a blend SBR/EPDM compound with high loading of Pliolite S6B(Styrene). This is a closed cell foam material with low density performed by compression molding extruded profiles then expanded with conventional ovens. I have been encountering problems with cracking of the surface and sides randomly. Does any one have any suggestions with out increasing the density?
I have been working on a blend SBR/EPDM compound with high loading of Pliolite S6B(Styrene). This is a closed cell foam material with low density performed by compression molding extruded profiles then expanded with conventional ovens. I have been encountering problems with cracking of the surface and sides randomly. Does any one have any suggestions with out increasing the density?