Structural
We have a project where upon removal of the forms there was one column that had significant voids at the top. Apparently, they had to use a sonotube form on this column and it blew out at the bottom during placement.
The other columns though are also showing cracking patterns that I have not seen before. To me they look like plastic shrinkage cracks, but these columns had steel forms that were left on for ~5-days after placement.
Reportedly the slump was ~5" and weather had been mild from the time it was poured until now. We have asked for photos of the columns as soon as the forms were removed but have not been provided.
I am seeking opinions on what may have caused these cracks. The contractor is saying these are completely normal.
The other columns though are also showing cracking patterns that I have not seen before. To me they look like plastic shrinkage cracks, but these columns had steel forms that were left on for ~5-days after placement.
Reportedly the slump was ~5" and weather had been mild from the time it was poured until now. We have asked for photos of the columns as soon as the forms were removed but have not been provided.
I am seeking opinions on what may have caused these cracks. The contractor is saying these are completely normal.