Hello there,
I apologize in advance if I am asking a question that has been answered elsewhere on the forum or is really easy to get the answer to - I am not a materials engineer and need some guidance.
We had a failure of a CS strainer bucket
- strainer nom dia 32"
- strainer body = forged CS
- service: mostly C1 @ 65 bar; C1 is clean, no H2o, no H2S, no HG
- op. temperature = 15-30°C, no fluctuations of the temperature or flow other than those caused by upstream mol sieve bed changever (dT = 8°C every 2.5h)
- there is a stopper ring inside the strainer, material SA-516-70 plate rolled the hard way and continuously fillet welded to the inside of the strainer body, purpose is prevent the strainer bucket from moving.
The strainer bucket was improperly installed (not tight against the stopper ring) which led to bucket rattling inside the strainer body and bucket failure.
This rattling also created 2 cracks on the stopper ring itself,
- location: on the edge of the fillet weld HAZ
- orientation: circumferential along the perimeter of the ring
- crack L = 30mm
- stopper ring t = 10mm, W = 75mm
We have already decided not to repair the strainer bucket, and NOT to return the bucket inside the strainer tee. We also have the following options:
1. Drill holes at the tips of the cracks to stop propagation of the cracks (difficult access for welded repair, need to isolate for hot work, needs time), or
2. Box up the strainer and start up the unit to avoid more downtime.
The questions are:
- Do we have to drill those holes regardless of whether the ring/cracks will be exposed to the load from the bucket or not? - What is the likelihood of those cracks propagating further through the ring if the strainer bucket (mechanical load) is removed? Ring failure would cause no concerns as its function is strictly to restrain the strainer bucket.
- In case of ring failure what is the likelihood of further crack propagation into the body (piping tee) of the strainer? Is this a credible scenario?
Thanks!
I apologize in advance if I am asking a question that has been answered elsewhere on the forum or is really easy to get the answer to - I am not a materials engineer and need some guidance.
We had a failure of a CS strainer bucket
- strainer nom dia 32"
- strainer body = forged CS
- service: mostly C1 @ 65 bar; C1 is clean, no H2o, no H2S, no HG
- op. temperature = 15-30°C, no fluctuations of the temperature or flow other than those caused by upstream mol sieve bed changever (dT = 8°C every 2.5h)
- there is a stopper ring inside the strainer, material SA-516-70 plate rolled the hard way and continuously fillet welded to the inside of the strainer body, purpose is prevent the strainer bucket from moving.
The strainer bucket was improperly installed (not tight against the stopper ring) which led to bucket rattling inside the strainer body and bucket failure.
This rattling also created 2 cracks on the stopper ring itself,
- location: on the edge of the fillet weld HAZ
- orientation: circumferential along the perimeter of the ring
- crack L = 30mm
- stopper ring t = 10mm, W = 75mm
We have already decided not to repair the strainer bucket, and NOT to return the bucket inside the strainer tee. We also have the following options:
1. Drill holes at the tips of the cracks to stop propagation of the cracks (difficult access for welded repair, need to isolate for hot work, needs time), or
2. Box up the strainer and start up the unit to avoid more downtime.
The questions are:
- Do we have to drill those holes regardless of whether the ring/cracks will be exposed to the load from the bucket or not? - What is the likelihood of those cracks propagating further through the ring if the strainer bucket (mechanical load) is removed? Ring failure would cause no concerns as its function is strictly to restrain the strainer bucket.
- In case of ring failure what is the likelihood of further crack propagation into the body (piping tee) of the strainer? Is this a credible scenario?
Thanks!