UCS-85 is a specific section of Sect. VIII, Div. 1 that addresses the required heat treatment of test specimens for UCS materials. What is the equivalent of this for UHA materials? For example, if a part will be solution-annealed (additional to SA by the mill) and requires a charpy test, does the coupon also need to be solution-annealed to match the part? It seems like it would make sense for the coupon to get the same heat treat, but I don't recall seeing this addressed anywhere in Sect VIII.