Mar 29, 2003 #1 JonLueke Mechanical Joined Mar 29, 2003 Messages 10 Location CA Hey all, What is a ballpark cost for extruding a small aluminum heat sink, no more than 50 cm long, 35 cm wide, and 20 cm wide? Or better yet, is there an online handbook that would have this information (or something similar)?
Hey all, What is a ballpark cost for extruding a small aluminum heat sink, no more than 50 cm long, 35 cm wide, and 20 cm wide? Or better yet, is there an online handbook that would have this information (or something similar)?
Mar 31, 2003 #2 ko99 Mechanical Joined Mar 3, 2003 Messages 211 Location US I'd guess tooling cost to be about $1200-2000, part cost about $2-4 depending on qty, finish, aspect ratio, flatness requirements, etc. I've used 8 or 10 heat sink extruders in the past. Let me know if you'd like any contact info. Kevin O'Connor http://www.ECooling.biz Upvote 0 Downvote
I'd guess tooling cost to be about $1200-2000, part cost about $2-4 depending on qty, finish, aspect ratio, flatness requirements, etc. I've used 8 or 10 heat sink extruders in the past. Let me know if you'd like any contact info. Kevin O'Connor http://www.ECooling.biz