I am trying to do a simple buckling analysis of a delrin pressure case using cosmoswork.
Case dimension:
OD: 8"
wall thickness: .4"
End cap thickness: .4"
Length: 2.625"
Material properties:
E: 2.83E+9 Pa
Yield stress: 8.9e+6 Pa
Poisson ratio: .3
Test load: 14.7 Psi
According to Roarks's Formulas the end cap should fail approx around 10m.
But the program give a load factor of 54 and the center of the end cap bulge outward rather than inward.
I am wondering wether I setup the analysis correctly? Any help or advice would be greatly appreciated.
Thanks
Case dimension:
OD: 8"
wall thickness: .4"
End cap thickness: .4"
Length: 2.625"
Material properties:
E: 2.83E+9 Pa
Yield stress: 8.9e+6 Pa
Poisson ratio: .3
Test load: 14.7 Psi
According to Roarks's Formulas the end cap should fail approx around 10m.
But the program give a load factor of 54 and the center of the end cap bulge outward rather than inward.
I am wondering wether I setup the analysis correctly? Any help or advice would be greatly appreciated.
Thanks