loony
Mechanical
- Feb 25, 2003
- 1
I use a machine who make's plastic film. The problem is that I have corrugations on the plastic film on the winding roll. The winding roll is in nip configuration with a contact roll.
Do you have any clues to solve that problem ?
thanks
Do you have any clues to solve that problem ?
thanks