I need advise about the best material for shielding the parents tube (90/10 CuNi tubes). What is the best for Cavitation resistant material available for sea water service and avoid galvanic reaction ? is AL-6XN, Titanium or 70/30 CuNi material?

 
Check out the Epoxy Polymeric coating systems.
 
You could try inserting ferrules in the tube ends. Many materials available including ceramics.

Good Luck
 
Hi
Titanium with tube inserts is the best solution. ssp