Corrosion resistance of Brass

Status
Not open for further replies.

Redpoint

Mechanical
Joined
Aug 11, 1999
Messages
11
Location
US
Does anyone know how yellow brass will hold up to phosphoric acid? I don't have that extensive of books which has that kind of information. Any help would be appreciated.
 
In general, the following materials, Al , cast iron, steel, brass and ferritic and martensitic stainless steel exhibit poor corrosion resistance in phosphoric acid.<br>
<br>
To be specific for 70-30 brass corrosion rate at 70 F 100% corrosive medium of phosphoric acid the corrosion rate is &gt; 0.05 mpy (mil per year) which is very poor and unacceptable in metallurgical sense.<br>
<br>
Type 316 austenitic Stainless steel will be a choice for phosphoric acid environment . It can be used up to 85%conc. and temperature up to boiling point with little attack.<br>
<br>
<br>
Regards,<br>
Surin Tan
 